MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Spartan EP 100
Categories: Fluid; Lubricant

Material Notes: Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickening, therefore increasing oil service life. SPARTAN EP oils contain a sulfur / phosphorus extreme pressure additive system that gives high load carrying ability and protection against wear. In addition these oils provide excellent protection against corrosion of steel and copper containing alloys. SPARTAN EP oils have good water handling properties: water separates from them rapidly preventing contamination of the system, and they are resistant to foam formation. SPARTAN EP oils can be used in either splash or circulating systems. SPARTAN EP gear oils are suitable for use wherever an industrial gear oil is required, and are particularly useful for use at high temperatures, up to 95°C. SPARTAN EP grades are suitable for the lubrication of heavily loaded enclosed gear sets including spur, helical and bevel designs and provide protection in applications where shock loading occurs. SPARTAN EP may also be used in worm gears, though a maximum temperature of 85°C is recommended for continuous operation. They may also be used for lubrication of plain bearings, and in rolling contact (anti-friction) bearings. They also find broad usage in marine gear applications.

Exxon SPARTAN EP gear oils are used in a wide range of industrial spur, helical, bevel and steel-on-steel worm gearing as well as marine applications. Specific applications include: Drives for conveyors, agitators, dryers, fans, mixers, presses, pulpers, pumps, screens, extruders, oil well pumps; Industrial bearings journal and rolling contact, especially operating at low speeds and high loads; Drives for main propulsion, centrifuges, deck machinery such as winches, windlasses, cranes, turning gears, pumps, elevators and rudder carriers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity Measurement 98Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 100 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 12 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 48ASTM D2783
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2783
Timken Test 65.0 lb
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 95.0 °C
Pour Point -27.0 °CASTM D97
Flash Point 235 °CASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
Demulsibility Time (min)30to 3 mL emulsion @ 82°C
Foam Sequence II, ASTM D8930/0
FZG Scuffing, DIN 5182, A/8.3/90, Fail Stage12+
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON227 / 75652

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.