MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips Marlex® 5619 LDPE Shrink and Heavy Duty Packaging Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: This low density polyethylene is tailored for blown film applications that require:
  • Superior strength
  • Good abrasion and tear resistance
  • Exceptional shrink and shrink tension
  • Low coefficient of friction
Typical blown film applications include:
  • Heavy duty packaging
  • Pallet shrink
  • Case shrink wrap
  • C&A film and container liners

Data provided by Chevron Chemical.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D1505
Water Vapor Transmission 10.0 g/m²/day0.644 g/100 in²/dayASTM F1249
Oxygen Transmission Rate 3500 cc/m²/day225 cc/100 in²/dayASTM D3985
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1500 ppm1500 ppm
Slip Level 400 ppm400 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 220 %220 %ASTM D882
Film Elongation at Break, TD 570 %570 %ASTM D882
Coefficient of Friction 0.130.13ASTM D1894
Elmendorf Tear Strength MD 245 g245 gASTM D1922
Elmendorf Tear Strength TD 215 g215 gASTM D1922
Dart Drop Test 225 g0.496 lbASTM D1709
Film Tensile Strength at Break, MD 27.0 MPa3920 psiASTM D882
Film Tensile Strength at Break, TD 27.0 MPa3920 psiASTM D882
1% Secant Modulus, MD 203 MPa29500 psiASTM D882
1% Secant Modulus, TD 238 MPa34500 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °FASTM D3418
Vicat Softening Point 104 °C219 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 8.0 %8.0 %ASTM D1003
Gloss 100 %100 %at 60°; ASTM D 2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVVB0 / 20506

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.