MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

INEOS Styrolution 153F Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Empera® 153F is general purpose polystyrene with high heat resistance and good flow properties. Empera® 153F is free of internal lubricants, e.g. zinc stearate.
    Features:
  • Food Contact Acceptable
  • General Purpose
  • Good Flow
  • High Heat Resistance
Agency Ratings: EU 2002/72/EC

RoHS Compliant: Contact Manufacturer

    Processing Method:
  • Foam Extrusion
  • Injection Molding
  • Sheet Extrusion

Formerly sold under the Empera® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.10 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiH 358/30; ISO 2039-1
Tensile Strength at Break 52.0 MPa7540 psiISO 527-2/50
Elongation at Break 2.0 %2.0 %ISO 527-2/50
Tensile Modulus 3.30 GPa479 ksiISO 527-2/1
Flexural Strength 75.0 MPa10900 psi2.0 mm/min; ISO 178
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Thermal Conductivity 0.160 W/m-K1.11 BTU-in/hr-ft²-°FDIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FUnannealed; ISO 75-2/A
Vicat Softening Point 101 °C214 °FISO 306/B50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Edistir N 2380 Polystyrene
INEOS Styrolution Polystyrol 168 N GR 2 PS
Ineos Nova N5000MG Compact PS
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
BASF Pluracol® 1026 Molded Foam Polyol

PZZSTYR983 / 209784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.