MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

EOS Copper CuCP AMCM M 290 1kW
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Copper Alloy

Material Notes: Commercially pure copper for the EOS M 290 with 1 kW - customized by AMCM - designed to reach excellent conductivity properties. Suitable for a wide variety of applications.

Main Characteristics:

  • Commercially pure copper (> 99.95 % purity)
  • Excellent electrical and heat conductivity
  • Designed for an EOS M 290 with a 1 kW laser which is the AMCM M 290 1kW sold by AMCM GmbH
Typical Applications:
  • Electrical motors
  • Inductors
  • Variety of industry applications requiring excellent conductivity properties

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity <= 0.50 %<= 0.50 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 235 MPa34100 psias manufactured
 220 MPa
@Treatment Temp. 1000 °C,
Time 3600 sec
31900 psi
@Treatment Temp. 1830 °F,
Time 1.00 hour
heat treated in argon atmosphere, slow cooling with argon
Tensile Strength, Yield 165 MPa23900 psias manufactured
 110 MPa
@Treatment Temp. 1000 °C,
Time 3600 sec
16000 psi
@Treatment Temp. 1830 °F,
Time 1.00 hour
heat treated in argon atmosphere, slow cooling with argon
Elongation at Break 45 %45 %as manufactured
 50 %
@Treatment Temp. 100 °C,
Time 3600 sec
50 %
@Treatment Temp. 212 °F,
Time 1.00 hour
heat treated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 0.00000172 ohm-cm>= 0.00000172 ohm-cmas manufactured & heat treated; ASTM E1004-17
 
Descriptive Properties
Volume rate5.4 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS927 / 280587

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.