MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AKG Polymers Vision PP PPC BL1008 Polypropylene Copolymer Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.
Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineering, Construction, Horticulture, Electronics

Information provided by AKG Polymers BV

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 - 0.940 g/cc0.0325 - 0.0340 lb/in³Internal
Filler Content <= 6.0 %<= 6.0 %Internal
Melt Flow 8.0 - 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 - 12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 6460 - 64Internal
Flexural Modulus >= 0.900 GPa>= 131 ksiISO 178
Charpy Impact, Notched >= 0.780 J/cm²
@Temperature 23.0 °C
>= 3.71 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
Falling Dart Impact >= 8.83 J
@Temperature 23.0 °C
>= 6.51 ft-lb
@Temperature 73.4 °F
Internal
 
Descriptive Properties
Application Areaautomotive
ColorBlack
Non-virgin Polymer Content (%), Min95
ProcessInjection Molding
Specific Featureshigh impact

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mytex Polymers AS78L-GM Polypropylene, Rubber modified, Compounded
Overview of materials for Polypropylene, Mineral Reinforced
Overview of materials for Polypropylene with 10% Talc Filler
Domo Technyl® A 246M Nylon 66, Impact Grade, EH50
Celanese Zytel® ST801AHS NC010 PA66-HI

PVISION07 / 83603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.