MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® LX9029 NC Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9029 NC is a high viscosity, plasticized, heat- and light stabilized PA12 compound for extrusion and injection molding, especially suitable for the manufacturing of highly flexible tubes and hoses. The material based on PA12 absorbs only small amounts of water. Components made from this material therefore show excellent dimensional stability under changing ambient humidity. VESTAMID® LX9029 NC is supplied as cylindrical granules, ready for processing, in moisture-proof polyethylene bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Preliminary data sheet.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering, Sports and Lifestyle
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: UV / light / weathering
Electrical: Insulating
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion
Special Characteristics: Light-stabilized, U.V. stabilized, High heat resistant, High viscosity
Color: Natural color
Additives: Plasticizer

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Viscosity Number 150 cm³/gISO 307, 1157, 1628
 220 cm³/gCorrected; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.00700 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0110 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527
Tensile Stress 19.0 MPa
@Strain 50.0 %
ISO 527
Elongation at Break 320 %Nominal; ISO 527
Tensile Modulus 240 MPaISO 527
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
Type of failure: C; ISO 179/1eA
 110 kJ/m²
@Temperature 23.0 °C
Type of failure: P; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 166 °CISO 11357-1/-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °CInjection Molding; ISO 294
 220 °C
Mold Temperature 60.0 °CInjection Molding; ISO 294
 60.0 °C
Injection Velocity 200 mm/secInjection Molding; ISO 294
 
Descriptive Properties
Blue water consumption24.1 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential2.4 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 5.5 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 5.5 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7924 / 325056

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.