MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP1304E3 Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applications such as toys, electric appliances, packaging and thin walled parts.

Availability: Africa & Middle East and Asia Pacific

Uses:

  • Consumer Applications
  • Crates
  • Furniture
  • Industrial Applications
  • Packaging
  • Tool/Tote Box

Processing Method: Compounding and Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70ISO 868
Tensile Strength, Yield 4790 psiISO 527-2/1A/50
Elongation at Yield 9.0 %ISO 527-2/1A/50
Tensile Modulus 206000 psiISO527-2/1A/1
Flexural Modulus 193000 psi0.079 in/min; ISO 178
Charpy Impact, Notched 1.60 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 318 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 174 °FISO 75-2/B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP3155E3 Polypropylene Copolymer
ExxonMobil Mytex™ AN17K-01
ExxonMobil PP1222F Mineral-filled Homopolymer
ExxonMobil PP5722E1 Polypropylene Copolymer
ExxonMobil PPU0009F Polypropylene Impact Copolymer

PEX99434 / 175670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.