MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kleerdex Elson® 407AS DC Plate, Polycarbonate, Clear  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes:

Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792; DIN 53479
Water Absorption 0.30 %0.30 %ASTM D570; DIN 53495
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 64.7 MPa9380 psiASTM D638
Elongation at Break 100 %100 %ASTM D638; DIN 53455
Modulus of Elasticity 2.20 GPa319 ksiASTM D638; DIN 53452
Flexural Yield Strength 93.2 MPa13500 psiASTM D790; DIN 53455
Flexural Modulus 2.60 GPa377 ksiASTM D790; DIN 53457
Compressive Strength 85.3 MPa12400 psiASTM D695
Izod Impact, Notched 8.47 J/cm15.9 ft-lb/inASTM D256
Izod Impact, Unnotched (ISO) 83.4 kJ/m²39.7 ft-lb/in²JIS K7110
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+6 - 1.00e+8 ohm1.00e+6 - 1.00e+8 ohmASTM D257; DIN 53482
Static Decay 0.0010 sec0.0010 secElectrostatic Discharge; MIL D-81715B
Dielectric Constant 4.04.0ASTM D150; DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°FASTM C177
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FASTM D648
Flammability, UL94  HB
@Thickness 3.00 - 4.80 mm
HB
@Thickness 0.118 - 0.189 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58ASTM D542
Haze 1.27 %1.27 %ASTM D1003
Transmission, Visible 84 %84 %Transmittance; ASTM D1003
 
Descriptive Properties
Coating Layer Bond Strength100/100JIS D0202
Distinctness of image97.6
Pencil HardnessBJIS K5400

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
OJSC Plastic ABS 2020-31 ABS Plastic
OJSC Plastic ABS 2020-31 M ABS Plastic
NUDEC® PC Polycarbonate Sheet
SEKISUI SPI KYDEX® 410 ABS/PVC
Evonik Cyrolon® AR Polycarbonate Sheet

PKLEEQ01 / 48848

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.