MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyrocks Chemical EP8400S90F-J7 Polyolefin Cable Compound
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: EP8400S90F-J7 is a kind of low-smoke halogen-free flame retardant polyolefin material. EP8400S90F-J7 has excellent mechanical, electrical and processing properties, high flame retardant. This material does not emit halogen acid gas, toxic and corrosive gases.

Information provided by Polyrocks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ASTM D792
pH >= 5.0>= 5.0IEC 60754-2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ASTM D2240
Tensile Strength 13.5 MPa1960 psiIEC 60811-1-1
 13.8 MPa
@Temperature 100 °C,
Time 605000 sec
2000 psi
@Temperature 212 °F,
Time 168 hour
Aging; IEC 60811-1-2
Elongation at Break 173 %173 %IEC 60811-1-1
 175 %
@Temperature 100 °C,
Time 605000 sec
175 %
@Temperature 212 °F,
Time 168 hour
Aging; IEC 60811-1-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+15 ohm-cm1.50e+15 ohm-cmIEC 60093
 2.50e+14 ohm-cm
@Temperature 70.0 °C,
Time 605000 sec
2.50e+14 ohm-cm
@Temperature 158 °F,
Time 168 hour
Immersion; IEC 60093
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -25.0 °C-13.0 °FPass; IEC 60811-1-4
Smoke Density 5050Flaming; ASTM E-662
 160160Non-Flaming; ASTM E-662
Oxygen Index 40 %40 %ASTM D2863
 
Descriptive Properties
Electrical conductivity<2 µS/mmIEC 60754-2
Halogen acid gas0 mg/gIEC 60754-1
High Temperature Pressure0.3380°C×4h, IEC 60811-3-1
Toxicity1NES 713-1985

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPROCKS029 / 278537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.