Product Description: Sequel 1828 thermoplastic polyolefin is designed for automotive and heavy-truck applications that require energy management combined with excellent ductility and stiffness over a broad temperature range. This material exhibits excellent processability and dimensional stability. Typical Customer Applications: Exterior Applications, Bumpers Availability: North America Features: Ductile; Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Stiffness; High Energy Absorption Uses: Automotive Applications; Automotive Bumper; Automotive Exterior Parts Information provided by LyondellBasell Industries |