MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Isoflon PC Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Good impact resistance among transparent materials

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccDIN 53479
Water Absorption 0.15 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75ASTM D785
Tensile Strength 70.0 MPaDIN 53455
Elongation at Break 50 %DIN 53455
Tensile Modulus 2300 MPaDIN 53457
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmDIN 53482
Dielectric Constant 3.0
@Frequency 1000 Hz
DIN 53483
Dielectric Strength 28.0 - 30.0 kV/mmDIN 53481
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°CDIN 52328
Thermal Conductivity 0.210 W/m-KDIN 52612
Melting Point 220 °CDIN 53736
Maximum Service Temperature, Air 115 °CContinuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
Minimum Service Temperature, Air -60.0 °CContinuous; DIN 52612
Flammability, UL94 V-0
@Thickness 6.00 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Covestro Makrolon® 8325 Polycarbonate

PISOFL920 / 123308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.