MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Universal Wire Works ER317L Stainless Steel Bare Wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: The alloy content of this alloy is somewhat higher than the 316L particularly in molybdenum. ER317L is used for welding alloys of similar composition in severe corrosive environments where crevice and pitting corrosion are a concern. The low carbon content increases the resistance to intergranular corrosion without the use of stabilizers.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.00 - 0.030 %
Chromium, Cr 19 %
Iron, Fe <= 72 %As Remainder
Molybdenum, Mo >= 2.5 %
Nickel, Ni 9.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 266SC Polyvinyl Chloride Pastes - filler Polymers
A. Schulman POLYBLAK™ 2723Pm Premium Black Color Concentrate, 25% Carbon Black Based In HDPE
BASF Heligoen® Blue L 7080 Color Additive
Blue River Coatings Wood Primer
Evonik AQUA-CHEM® 896-0001 Aqueous Industrial Colorant

NUWW072 / 19622

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.