| Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offering excellent combination between mechanical properties and surface aspect. This grade is widely used for automotive part: outside mirror base plate. This product is available in black color and in colors on request. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |