MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Morgan Advanced Ceramics Insulating Firebricks JM 32 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: High Temperature Series

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc
@Temperature 23.0 °C
0.0452 lb/in³
@Temperature 73.4 °F
at 50% RH; ASTM C-134-84
Deformation 0.20 %
@Temperature 1370 °C,
Time 5400 sec
0.20 %
@Temperature 2500 °F,
Time 1.50 hour
Hot Load Strength, 0.069 Mpa; ASTM C-16
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00210 GPa
@Temperature 23.0 °C
0.305 ksi
@Temperature 73.4 °F
at 50% RH; ASTM C-93-84
Compressive Strength 3.50 MPa508 psiCold Crushing Strength, 50% RH; ASTM C-93-84
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.490 W/m-K
@Temperature 400 °C
3.40 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.500 W/m-K
@Temperature 600 °C
3.47 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.510 W/m-K
@Temperature 800 °C
3.54 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.530 W/m-K
@Temperature 1000 °C
3.68 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 0.560 W/m-K
@Temperature 1200 °C
3.89 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 0.600 W/m-K
@Temperature 1400 °C
4.16 BTU-in/hr-ft²-°F
@Temperature 2550 °F
Shrinkage 0.60 %
@Treatment Temp. 1730 °C,
Time 86400 sec
0.60 %
@Treatment Temp. 3150 °F,
Time 24.0 hour
after soaking; ASTM C-210
 
Component Elements PropertiesMetricEnglishComments
Al2O3 77 %77 %
Fe2O3 0.30 %0.30 %
SiO2 21.5 %21.5 %
 
Descriptive Properties
Classification Temperature (°C)1760
Reversible Linear Thermal Expansion Max (%)1.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Morgun AL Thermal Ceramic

CMORF6022 / 202806

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.