Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance. Available in: North America Product Applications: TECHNYL ® a 218W V15 is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water: e.g. electro-magnetic valves. This product is available in natural. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |