MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 7545 Urethane Adhesive, 7545-E Curative Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7545 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive also bonds primed metals and various combinations of dissimilar substrates. LORD 7545 adhesive system is available in a range of working times to accommodate a wide variety of process requirements. After opening, protect adhesive from excessive exposure to moisture by installing desiccant cartridges and/or using dry nitrogen as an inert cover.

Features: demonstrates high strength and excellent durability for structural applications. exceeds U.S. DOT requirements for non-flammability and does not require explosion-proof equipment. off-white color of cured adhesive provides an acceptable appearance when non-painted or visible. does not contain ozone depleting chemicals. resists sunlight, weathering, humidity and salt spray. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 - 1.32 g/cc0.0459 - 0.0476 lb/in³
Solids Content 100 %100 %by weight, mixed with curative
Brookfield Viscosity 230000 - 650000 cP
@Temperature 25.0 °C
230000 - 650000 cP
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °Fclosed cup
 
Processing PropertiesMetricEnglishComments
Pot Life 120 - 180 min
@Temperature 24.0 °C
120 - 180 min
@Temperature 75.2 °F
time to handling strength, mixed with resin
Working Life 22.0 - 38.0 min
@Temperature 24.0 °C
22.0 - 38.0 min
@Temperature 75.2 °F
working time, mixed with resin
Shelf Life 6.00 Month
@Temperature 18.0 - 30.0 °C
6.00 Month
@Temperature 64.4 - 86.0 °F
in original, unopened container
 
Descriptive Properties
AppearanceOff-White Paste
Mix Ratio1 to 0.85by weight, resin to curative
 1 to 1by volume, resin to curative
Processing Time30 min.Purge time, 24 C, mixed with Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9133 / 232521

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.