MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis Queo™ 6201LA-P Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Queo 6201LA-P is an ethylene based octene-1 elastomer, produced in a solution polymerization process using a metallocene catalyst. The material is powdered with talcum to prevent sticking of the pellets. CAS-No. 26221-73-8

Special Features:

  • Outstanding low temperature impact in Automotive and Construction TPOs
  • Polymer modifier in various polymer blends
Applications:
  • Automotive and Construction TPO
  • EPDM profile and cable manufacturing
  • EPDM replacement / TPV / grafting
Additives: Queo 6201LA-P contains a low amount of processing stabilizers. The material is powdered with talcum to prevent sticking of the pellets.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.862 g/ccISO 1183
Viscosity 100 cP
@Shear Rate 100 1/s,
Temperature 230 °C
 140 cP
@Shear Rate 100 1/s,
Temperature 190 °C
 220 cP
@Shear Rate 100 1/s,
Temperature 140 °C
 500 cP
@Shear Rate 0.100 1/s,
Temperature 230 °C
 1200 cP
@Shear Rate 0.100 1/s,
Temperature 190 °C
 3400 cP
@Shear Rate 0.100 1/s,
Temperature 140 °C
Mooney Viscosity 31.0
@Temperature 100 °C
(1+4); DIN 53523-3:1976
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 61.0ISO 868
Hardness, Shore D 16.0ISO 868
Elongation at Break >= 800 %ISO 527-2
Tensile Modulus 4.00 MPaASTM D638-T4
Izod Impact, Notched (ISO) NBISO 180:2000
 
Thermal PropertiesOriginal ValueComments
Melting Point 49.0 °CISO 11357-3
Brittleness Temperature <= -90.0 °CISO 974

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9893 / 323250

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.