MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vinnolit® E 75 HV PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 75 HV PVC for paste application. Vinnolit® E 75 HV is a fine-particle sized, paste-making emulsion homopolymer, classified as high viscosity resin. Plastisols made with Vinnolit® E 75 HV exhibit pseudoplastic rheology Vinnolit® E 75 HV is particularly suitable for the production of compact films and chemically blown foams. Typical application is artificial leather, especially for thermoformed surfaces in the automotive applications. Vinnolit® E 75 HV is also suitable for technical coatings yielding plastisols of medium-high viscosity and very good compatibility with bonding agents. Moreover, Vinnolit® E75 HV remarkably increases the gelling force of plastisols. Plastisols based on Vinnolit® E 75 HV can be applied by all commonly used coating techniques for leather cloth. Vinnolit® E 75 HV is particularly suitable for the manufacture of artificial leather cloth that is subjected to thermoforming.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.35 %<= 0.35 %ISO 1269
Apparent Bulk Density 0.420 g/cc0.0152 lb/in³ISO 60
Particle Size <= 63 µm<= 63 µm<= 2.0% Retained on 0.063 mm Sieve; DIN EN ISO 53195
 
Descriptive Properties
Emulsifier ContentMedium
Fogging Characteristic (gravimetric)<=1.5 mgDIN EN ISO 75201 B
K-Value73ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO932 / 291129

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.