MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow ISONATE™ 50 O,P` Pure MDI
Categories: Fluid

Material Notes: ISONATE™ 50 O,P` is a high ortho-para MDI designed for use in polyurethane adhesives, sealants, sports flooring, coatings, electrical encapsulants and flexible molded foams. ISONATE™ 50 O,P` offers formulators a slower reactivity and increased amorphous character for improved handling and longer pot life. In prepolymer formulation, it results in lower viscosity and improve shelf stability.

50% 4,4-diphenylmethane diisocyanate and 50% 2,4-diphenylmethane diisocyanate

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.204 g/cc
Density 1.20 g/cc
Viscosity 10 cP
Vapor Pressure <= 0.000100 torr
@Temperature 43.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.0030% as HCl
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.80 J/g-°C
Melting Point 68.0 °F
Boiling Point 314 °C
Decomposition Temperature 230 °C
Flash Point >= 177 °CP.M.C.C.; ASTM D93
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Hydrolyzable Chloride ppm18
Isocyanate Equivalent Weight125.5
NCO Content wt%33.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ISONATE™ 181 MDI Prepolymer
Dow ISONATE™ 125M Pure MDI
Dow ISONATE™ 240 MDI Prepolymer
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
Resin Technology Group 404 Oxy-Bond™ Electrically Conductive Epoxy Adhesive

PDOW1392 / 30610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.