MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
OJSC Plastic ABS 15F ABS Impact and Heat Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; ABS Polymer

Material Notes: Used to provide impact strength and heat resistance of the compositions of PVC alone or in mixture with other modifiers: chlorinated PE, acrylic modifiers, a methyl methacrylate butadiene styrene modifiers. The product is combined with rigid PVC and the additives for processing (waxes, fillers, lubricants, stabilizers, etc.) Has a stabilizing effect for the compositions of PVC. An additional feature is the stability of the mechanical properties of PVC profiles at low temperatures, improving the heat resistance.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.290 - 0.380 g/ccGOST 11035.1-93
Density 1.04 g/ccGOST 15139-69
Melt Flow >= 17 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Clause 7.2 of TU and GOST 11645-73
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100 - 110GOST 24622-91
Elongation at Break 18 %GOST 11262-80
Modulus of Elasticity 1.90 - 2.00 GPaGOST 9550-81
Izod Impact, Notched (ISO) >= 7.00 kJ/m²
@Temperature -30.0 °C
GOST 19109-84
 7.00 kJ/m²
@Temperature -30.0 °C
GOST 19109-84
 >= 13.0 kJ/m²
@Temperature 23.0 °C
Clause 7.3 of TU and GOST 19109-84
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 97.0 °CGOST 12021-84
Vicat Softening Point >= 100 °Cload 50N; Clause 7.4 of TU and GOST 15088-2014
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %Clause 7.5 of TU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POJSC970 / 192486

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.