MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol PEARLSTICK™ 5707 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5707 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU).

Description: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.

Uses: Synthetic leather and magnetic media binder, inks and screen printing, films for lamination.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D-792
Viscosity 85000 cP
@Temperature 204 °C
Melt; ASTM D-1084-88
Brookfield Viscosity 600 cP15% T.S. in THF
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D-2240
Hardness, Shore D 45ASTM D-2240
Tensile Strength 50.3 MPaASTM D-412/D-638
Elongation at Break 380 %ASTM D-412/D-638
100% Modulus 9.70 MPa
@Strain 100 %
ASTM D-412/D-638
300% Modulus 34.5 MPa
@Strain 300 %
ASTM D-412/D-638
Peel Strength 0.0400 kN/mAdhesion to PET; TP-141
 0.400 kN/mT-peel, Aluminum Foil; ASTM D-1876-72
 2.30 kN/mT-peel, Mylar Film; ASTM D-1876-72
 
Thermal PropertiesOriginal ValueComments
Softening Point 92.0 °CKoefler; ASTM D-1525
Glass Transition Temp, Tg -3.00 °C
Ring & Ball Softening Point 187 °CASTM E-28-92
 
Descriptive Properties
Gradient Bar Tack Temperature161°C
Open Time<5 secASTM D-4497-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5054 / 238924

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.