MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK 25-20 Cast UNS J94224 Heat Resistant Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: Increased strength for more highly stressed applications. Good resistance to oxidizing or reducing process flow.

Applications: Calcining tubes, pier caps, high temperature fixtures and hardware.

Information provided by MetalTek

Key Words: Cast UNS J94224; Cast Grade HK; Cast ASTM A297, A608; Wrought UNS S31000; Wrought Grade 310
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Tensile Strength, Ultimate >= 450 MPa>= 65300 psi
Tensile Strength, Yield >= 240 MPa>= 34800 psi
Elongation at Break >= 10 %>= 10 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1025 °C1877 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 - 0.60 %0.20 - 0.60 %
Chromium, Cr 24 - 28 %24 - 28 %
Iron, Fe 45.4 - 57.8 %45.4 - 57.8 %As Balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 18 - 22 %18 - 22 %
Silicon, Si <= 2.0 %<= 2.0 %
 
Descriptive Properties
Heat TreatmentNot Heat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
310 Stainless Steel, annealed strip
310 Stainless Steel, annealed sheet
AISI Type 310S Stainless Steel
AISI 310 Cast Stainless Steel, UNS J94302

NMETEK092 / 18342

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.