MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Akro-Plastic Akrotek® PK-VM GF 60 (4923) PK Conditioned, 60% Glass Filled
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: The renaissance of this polymer came about with an environmental program aimed at reducing greenhouse gases. The comonomer is CO (carbon monoxide), an industrial „waste” gas, which forms an unusual product when bonding with the polymer. The terpolymer, which forms the basis of most AKROTEK® PK formulations when using the monomers ethylene and propylene, currently has the greatest significance. AKRO-PLASTIC GmbH produces two product families from this base polymer (HM = normal flow and VM = very easy-flowing), based on the former portfolio of the Shell AG, from non-reinforced to high-glass-fibre-reinforced standards, from flame-retardant to carbon-fibre-reinforced custom grades

The characteristic properties of these properties include:

  • excellent dynamic resilience
  • good barrier properties
  • good tribological properties
  • high resistance to chemicals
  • good hydrolysis resistance
  • shorter cycle times
Application areas:
  • Industry
  • Automotive industry
  • Electronics/Electrical

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Filler Content 60 %60 %ISO 1172
Moisture Absorption 0.30 - 0.40 %
@Temperature 70.0 °C
0.30 - 0.40 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psi5 [mm/min]; ISO 527-2
Elongation at Break >= 1.5 %>= 1.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 17.3 GPa2510 ksi1 [mm/min]; ISO 527-2
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Akro-Plastic Akromid® B3 GF 60 1 black (2489) PA6, Conditioned, 60% Glass Filled
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass
Overview of materials for AISI 9000 Series Steel
Akro-Plastic Akrotek® PK-VM GF 60 (4923) PK Dry, 60% Glass Filled

PAKRO148 / 182735

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.