MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M 6146 Kraft Medium Duty Reinforced Water Activated Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ Medium Duty Reinforced Water Activated Tape 6146 Kraft is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and high tack water activated adhesive system.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 165 microns6.50 milCaliper; ASTM D645
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Break, MD 63.6 - 68.9 MPa9220 - 9990 psi
Film Tensile Strength at Break, TD 26.5 - 31.8 MPa3840 - 4610 psi
 
Descriptive Properties
Adhesive TypeHigh Tack, Water Activated, modified Starch Based Adhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34161 / 168908

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.