MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lanxess LEWATIT® VP OC 1026 Macroporous Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® VP OC 1026 is a macroporous resin based on a styrene-divinylbenzol copolymer containing di-2-ethylhexyl phosphate (D2EHPA). This extracting agent is already included directly during the polymerization, which leads to a high concentration of the active ingredient. In addition, a loss of extractant during operation is minimized (as long as they pH of the process solution as well as rinse water is kept below pH 4). Cations are adsorbed by Lewatit VP OC 1026 in the following order: Ti4>Fe3>In3>Sn2,4>Sb3>Bi3>Vo2>Be2>Al3>Zn2>Pb2>Cd2>Ca2>Mn2>Cu2>Fe2>Co2>Ni2>Mg2>Cr3>>Alkali. Fields of application: It can generally be assumed that Lewatit UP OC 1026 those components receives from aqueous solutions, which can be removed by means of the liquid extractant D2EHPA from sulfur and hydrochloric acid solutions as a function of pH, eg.:
  • divalent ions of zinc, uranium (UO2), vanadium (VO)
  • trivalent ions of lanthanides, indium, iron, aluminum
  • tetravalent ions of actinides, titanium
Advantages of Lewatit VP OC 1026 compared to solvent extraction:
  • no organic solvent required
  • no phase separation problems
  • simple equipment similar to conventional bead type ion exchange resins
Important hints for application: There is a marked distinction in its physical and chemical properties from those of the known ion exchange resins. It has to be emphasized that: the active ingredient of Lewatit VP OC 1026 is in the form of the acid ester. This means that the form supplied can be directly used. Exposure to sodium hydroxide or sodium carbonate should be avoided since the active ingredient will be displaced from the resin. Also the pH of process solution and rinse water should be always be < pH 4. The resin is floating to the liquid surface. Therefore the column should be equipped with an adequate distribution plate at the column’s head and be operated upstream. Due to the specific method of manufacturing the resin has a relatively high percentage of fine beads. Therefore it is recommended to use inert resin (Lewatit IN 42) to protect the head distributor against plugging. To protect the bottom distributor a gravel layer can be applied. Backwash can only be carried out in down flow mode by means of an acidic, in minimum 4% slat containing solution. Backwash water is discharged through a special out pipe positioned below the ion exchange bed. The resin can be used without backwashing only in the case that a through – pre filtration is carried out. In this case the column is designed with a packed bed.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Density 0.970 g/cc0.0350 lb/in³
Bead Size 0.315 - 1.60 mm0.0124 - 0.0630 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6063-O
Goodfellow Titanium Diboride, TiB2
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
Wacker Vinnapas® CA54 Vinyl Acetate Ethylene
Titanium Boride, TiB2

PLANY8860 / 209252

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.