MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Buna SE 1721 TE Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Buna SE 1721 TE is a butadiene-styrene copolymer, produced by cold emulsion polymerization, using fatty and rosin soaps as emulsifiers. The elastomer is extended in oil with a PCA (Polycyclic Aromatic Hydrocarbons) content less than 3.0% and PAHs (individual Polycyclic Aromatic Hydrocarbons) content less 10 ppm which is compliant the European directive 2005/69/EC. The monomers are randomly distributed in the polymer structure, while the butadiene fraction is found in its major part in the trans configuration with small fractions of cis and vinyl configurations.

CAS No: 9003-55-8

Plant: Duque de Caxias-RJ-Brazil

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %ASTM D5668
Mooney Viscosity 5555[ME]; ASTM D1645
 
Chemical PropertiesMetricEnglishComments
Styrene Content 40 %40 %Bound; ASTM D5775
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature <=40.0 °C
12.0 Month
@Temperature <=104 °F
 
Descriptive Properties
Content<0.5 %Free soap
 27.2 percentOil
 5 percentOrganic acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tipco Tipcofil® KMX 800 FR - UL94-V0 Flame Retardant, Highly Filled PBT/PC Alloy, with High Heat Stability
Synthos BUNA™ SB 1723 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Process Technologies Inc BUNA-N Sanitary Gasket
Lanxess Buna CB 55 L Rubber
Dow Buna® SB 1500 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PLANY8514 / 208907

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.