MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

High-Leaded Tin Bronze, UNS C93400, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Casting Yield, Fluidity; Medium –Gassing, Effect of Section Size; Low - Drossing, Shrinkage in Solidification

Fabrication Properties: Good Suitability – Brazing, Soldering

Typical uses: Washers; Bearings; Bushings; Corrosion Resistant Castings; Pump Impellers; Slide Bars

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 60
@Load 500 kg
60
@Load 1100 lb
Tensile Strength >= 172 MPa>= 25000 psi
 221 MPa32000 psiTypical
Tensile Strength, Yield >= 82.7 MPa>= 12000 psi
 110 MPa16000 psiTypical, 0.5% Ext
Elongation at Break >= 8.0 %>= 8.0 %
 20 %20 %Typical
Tensile Modulus 75.8 GPa11000 ksi
Compressive Strength 331 MPa48000 psi0.1 in. set/in.
Fatigue Strength 103 MPa
@# of Cycles 1.00e+8
15000 psi
@# of Cycles 1.00e+8
Machinability 70 %70 %
Izod Impact 6.78 J5.00 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000143 ohm-cm0.0000143 ohm-cm12% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 4.84 W/m-K33.6 BTU-in/hr-ft²-°F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.50 %<= 0.50 %
Copper, Cu 82 - 85 %82 - 85 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb 7.0 - 9.0 %7.0 - 9.0 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.50 %<= 0.50 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 7.0 - 9.0 %7.0 - 9.0 %
Zinc, Zn <= 0.80 %<= 0.80 %
 
Descriptive Properties
Proportional Limit8 ksi

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC93400x2 / 293224

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.