MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Inorganic Wet Felt 2300-W Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Inorganic Wet Felt is a damp, insulating sheet material based on our inorganic vacuum formed product formulations. Our engineered blend of long and short fiber ensures the optimum strength and flexibility of product during installation. Often used as a form-fitting material, Inorganic Wet Felt is ideal for installations that have uncertain dimensions or complex surface geometry. Inorganic Wet Felt is water-based and can simply be hand-moulded into place and air dried. Thinner sheets are supplied in rolls, whereas thicker sheets are supplied flat. Stringent process controls ensure that Inorganic Wet Felt is provided at the optimum moisture content and strength.

Applications:

  • Wrapping exhaust manifolds in marine engines
  • Wrapping fuel injector nozzles in solid fuel fired kilns
  • Lining combustion duct work in incinerators and boilers
  • Lining hot tuyers in upcomers of blast furnaces
  • Hand packed to protect the anchor of an element hanger module.

Information provided by Morgan Advanced Materials

Key Words: thermal ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.272 g/cc0.00983 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000390 GPa0.0566 ksi
Compressive Strength 0.0500 MPa7.25 psiat 5% compression
 0.0600 MPa8.70 psiat 10% compression
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.13 J/g-°C0.270 BTU/lb-°F
Thermal Conductivity  0.0700 W/m-K
@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.100 W/m-K
@Temperature 538 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 0.150 W/m-K
@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1500 °F
 0.220 W/m-K
@Temperature 1093 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1999 °F
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air <= 1260 °C<= 2300 °FContinuous Use
Shrinkage  0.19 %
@Treatment Temp. 982 °C
0.19 %
@Treatment Temp. 1800 °F
 0.30 %
@Treatment Temp. 816 °C
0.30 %
@Treatment Temp. 1500 °F
 2.7 %
@Treatment Temp. 1093 °C
2.7 %
@Treatment Temp. 1999 °F
 3.4 %
@Treatment Temp. 1204 °C
3.4 %
@Treatment Temp. 2199 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 32 %32 %
SiO2 68 %68 %
 
Descriptive Properties
Colorwhite
Maximum Gas Velocity (m/sec)61

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Inorganic Wet Felt 2600-W Thermal Ceramic
Morgan Advanced Ceramics Kaoclad™ 1260 Thermal Ceramic
Morgan Advanced Ceramics Kaoclad™ 1400 Thermal Ceramic
MetalTek MTEK 29-4 Cast UNS J92605 Heat Resistant Stainless Steel
MetalTek MTEK HC-225 UNS F45005 Abrasion Resistant Cast Iron

CMORF6008 / 202792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.