MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Features

Chevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined, select high viscosity index base oils, and a lithium complex soap. It is red in color and smooth and stringy in texture. Chevron RPM Automotive LC Grease EP NLGI 2 is for use in normal ambient temperatures

Applications

Chevron RPM Automotive LC Grease EP is recommended for:

  • general use in the lubrication of trucks, tractors, and passenger cars. This includes ball joints, universal joints, and all other chassis points, wheel bearings, water pumps, and fifth wheels.
  • boat trailer wheel bearings
  • high temperature disc brake bearing applications

It is approved for the NLGI Certification Mark GC-LB.

Chevron RPM Automotive LC Grease EP is registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Key Words: CPS Number: 226454; MSDS Number: 7655
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9090Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 914 SUS914 SUS
Saybolt Viscosity at 210°F 82 SUS82 SUS
Kinematic Viscosity at 40°C (104°F) 173 cSt173 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.5 cSt15.5 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)Weld Point
Four Ball Wear 0.500 mm0.0197 in
Penetration 280280Worked
Penetration P(0), 1/10 mm 267267
Timken Test 18100 g40.0 lb
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -18.0 °C-0.400 °F
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 198 °C388 °FASTM D92
Dropping Point 270 °C518 °F
 
Descriptive Properties
ColorDark Green
TextureSmooth, Buttery
Thickener, % / type12 / Lithium Complex

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV260 / 74875

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.