Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" depth, then air set for 2-4 hours and cured at 200 ºF prior to operation. Two-part systems are used to produce high temperature molds and fixtures. |
Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |