MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset

Material Notes: Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.

Key features and benefits are:

  • Supports ANSI Z124.2 and CSA B45.5 requirements
  • High gloss surface appearance with minimal rippling on deep draws
  • Excellent as-molded dimensional tolerances
  • Outstanding moldability and flow in compression molding processes
  • Standard colors are white and bone
  • Designed for compression molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.76 g/cc
Linear Mold Shrinkage 0.0020 cm/cmPolymerization Shrinkage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaASTM D638
Tensile Modulus 10.0 GPaASTM D638
Flexural Strength 128 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Poissons Ratio 0.30
Shear Modulus 3.80 GPaCalculated
Izod Impact, Notched 530 J/mASTM D256
Izod Impact, Unnotched 7.00 J/cmASTM D4812
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°CXY Direction
Thermal Conductivity 0.300 W/m-K
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °CCompression Molding
Clamp Pressure 500 - 1000 psiMolding Pressure
 
Descriptive Properties
Flame Resistancepass at 3 mmANSI Z124.2
Stain ResistancepassANSI Z124.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC

PPREMH976 / 140374

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.