MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: 45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Water Absorption at Saturation 4.9 %4.9 %ISO 62
Linear Mold Shrinkage 0.0015 - 0.0040 cm/cm0.0015 - 0.0040 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 210 MPa30500 psiISO 527
Elongation at Break 2.8 %2.8 %ISO 527
Tensile Modulus 14.2 GPa2060 ksiISO 527
Flexural Strength 280 MPa40600 psiISO 178
Flexural Modulus 11.4 GPa1650 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Dielectric Strength 65.0 kV/mm1650 kV/inIEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FISO 11357
Maximum Service Temperature, Air 110 °C230 °FContinuous use
 200 °C392 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYR816 / 126615

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.