MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

PoolKemie RESINPOL R 302 Polyester resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Unsaturated isophthalic acid based polyester resin, dissolved in styrene, thixotropic and pre-accelerated. This resin combines excellent mechanical and chemical resistance with good temperature resistance. Good application characteristics and excellent capacity for impregnating reinforcement.

Application: This product is suitable for the construction of boats, storage tanks, ducts for the chemical and sanitary industries, and other applications requiring special mechanical or chemical resistance. R.302 resin is also suitable for making containers and other items for the wine and food industries, and for any element that comes into contact with products destined for human consumption.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.20 g/cc1.00 - 1.20 g/ccSystem Characteristics
 1.10 - 1.30 g/cc1.10 - 1.30 g/ccCured
Solids Content 50 - 54 %50 - 54 %PK04
Brookfield Viscosity 400 - 600 cP400 - 600 cP(9.8 sec-1) PK01
 1400 - 2200 cP1400 - 2200 cP(0.98 sec-1) PK01
Linear Mold Shrinkage 0.0029 - 0.0035 cm/cm0.0029 - 0.0035 in/inCured
Storage Temperature <= 20.0 °C<= 68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 40 - 4440 - 44Cured; ASTM-D 2583
Elongation at Break 3.6 - 4.0 %3.6 - 4.0 %Cured; UNI EN 61
 
Processing PropertiesMetricEnglishComments
Gel Time 8.00 - 14.0 min8.00 - 14.0 minPK02
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Exothermic peak19-24 mintime, PK02
 195-215°CTemperature, PK02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOOLK060 / 318539

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.