MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
EBS ACRAMAXX M10-6 Structural Methacrylate Adhesive
Categories: Polymer; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ACRAMAXX M10 series structural adhesives are based on methacrylate adhesives and formulated for superior metal bonding performance. The M10 adhesives were developed to withstand post bake oven temperatures up to 380°F (194°C) for up to 30 minutes. The M10 adhesives are available in two working times, M10-6A or M10-18A (Component A). These two adhesive components are formulated to be mixed with a single activator M10-1BNAT (Component B) at a 10:1 mix ratio. These products are designed with fast cure times and high strength to adhere to assemblies of thermoset composites, plastics, and are formulated to be primerless on most metal surfaces.

Bonds to Polyesters, vinyl esters, SMC, epoxies, acrylics, PVC/FPVC/CPVC, polycarbonate, ABS, styrenics, stainless steel, carbon steel, aluminum, coated metals, galvanized metals, and many other composites, thermoplastics, and metals. Does not bond well to polyolefins, TPO, acetal, or fluoropolymers.

Information provided by Engineered Bonding Solutions, LLC (EBS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.018 g/ccComponent A
 1.189 g/ccComponent B
Viscosity 80000 - 120000 cPComponent B
 300000 - 500000 cPComponent A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2900 psiPostcured
Elongation at Break 10 - 20 %Postcured
Modulus of Elasticity 175 ksiPostcured
Adhesive Bond Strength 3100 psiLap Shear, CRS (lightly sanded), post-cured; Bake 30min @380°F; ASTM D1002
 3100 psiLap Shear, Al (as received), post-cured; ASTM D1002
 3100 psiLap Shear, Al (as received), post-cured; Bake 30min @380°F; ASTM D1002
 3100 psiLap Shear, CRS (lightly sanded), post-cured; ASTM D1002
 3100 psiLap Shear, SS304 (as received), post-cured; ASTM D1002
 3100 psiLap Shear, Galvanneal (as received), post-cured; Bake 30min @380°F; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °Ccontinuous
 121 °Cintermittent
Minimum Service Temperature, Air -55.0 °Cintermittent
 -40.0 °Ccontinuous
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 14.0 minFixture Time
Working Life 6.00 min
Shelf Life 6.00 Month
 
Descriptive Properties
ColorCreamComponent A
 NaturalComponent B
Mix Ratio ( By Volume)10 to 1A:B
Mix Ratio ( By Weight)8.6 to 1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEBS990 / 287722

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.