MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Corr-Paint™ CP2080 High Temperature Protective Coating Novolac-Epoxy, Unfilled
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Two-part, clear, Novolac-epoxy with exceptional abrasion and corrosion resistance for continuous operations to 300ºF (150ºC) and intermittent use to 400ºF (204ºC).

Vendors: Aremco offers a wide range of ceramic, epoxy, urethane, and silicone sealers for thermal spray applications from 300°F (150°C) to 3000°F (1650°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Solids Content 100 %weight
 100 %volume
Volatile Organic Compounds (VOC) Content 0.00 g/l
Viscosity 600 - 1000 cPMixed Viscosity
Thickness 1.00 milestimated wet film thickness
 1.00 milrecommended dry film thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Flash Point >= 200 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 90.0 °FApplication Temperature
Cure Time 2.00 hour
@Temperature 150 °C
Option B. 8 Hour Air Set Prior to Curing
 24.0 hour
@Temperature 22.2 °C
Option A. 8 Hour Air Set Prior to Curing
Shelf Life 12.0 Month
@Temperature 23.0 °C
 
Descriptive Properties
ColorClear
Dry Film Coverage ft2/gal1604at 1 mil
Mix Ratio100:40by weight
 2:1by volume
ThinnerXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAREM70c / 256039

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.