MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Elements Silicon Carbide Nanoparticles
Categories: Ceramic; Carbide

Material Notes: General Description

Silicon Carbide (SiC) Nanoparticles, whiskers, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Carbide Particles are typically 10 - 150 nanometers (nm) with specific surface area (SSA) in the 10 – 75 m 2 /g range. Nano Silicon Carbide Particles are also available in ultra high purity and high purity and coated and dispersed forms. Research into applications for Silicon Carbide nanocrystals includes use as a dielectric coating, in solar cell applications, as a high temperature insulator, as a gas sensor and for use in other coatings, plastics, polymers and wire.

Key Words: Formula: SiC; CAS Number: 409-21-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.010 - 0.15 µm
Specific Surface Area 10 - 75 m²/g
 
Descriptive Properties
AppearanceSilvery

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics Kao-Tex 2200 AT-21 Sewing Thread
American Elements Silicon Nanoparticles
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 Ferritic Stainless steel
3M Techical Ceramics Ekasic® T Plus Silicon Carbide

EJAMER73 / 5556

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.