MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wittenburg Cawiton PR13620 SEBS, Medical Grade
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Cawiton PR13620 is a medical grade SEBS compound with a hardness of 20 Shore A. This grade is suitable for injection molding and profile extrusion.

Application: Medical grade

Information provided by Wittenburg Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 2781
Melt Flow 1.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20
@Time 3.00 sec
20
@Time 0.000833 hour
ISO 868
Tensile Strength 1.90 MPa276 psiFlow direction; ISO 37
 3.30 MPa479 psiCross Flow direction; ISO 37
Elongation at Break 470 %470 %Flow direction; ISO 37
 880 %880 %Cross Flow direction; ISO 37
100% Modulus 0.400 MPa58.0 psiCross Flow direction; ISO 37
 0.900 MPa131 psiFlow direction; ISO 37
200% Modulus 0.600 MPa87.0 psiCross Flow direction; ISO 37
 1.20 MPa174 psiFlow direction; ISO 37
300% Modulus 0.800 MPa116 psiCross Flow direction; ISO 37
 1.40 MPa203 psiFlow direction; ISO 37
Tear Strength, Total 9.10 N2.05 lb (f)Cross Flow direction; ISO 34-2
 9.40 N2.11 lb (f)Flow direction; ISO 34-2
Compression Set 26 %26 %ISO 815
 
Thermal PropertiesMetricEnglishComments
Melting Point 151 °C304 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 60.0 °C86.0 - 140 °FHopper
Rear Barrel Temperature 170 - 200 °C338 - 392 °F
Middle Barrel Temperature 180 - 210 °C356 - 410 °F
Front Barrel Temperature 190 - 220 °C374 - 428 °F
Nozzle Temperature 190 - 230 °C374 - 446 °F
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWITTN001 / 281751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.