MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Extruded

Material Notes: Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 masterbatch accelerates the moisture-induced crosslinking reaction and imparts track resistance, resistance to degradation by ultraviolet light stability to the final product.

Visico ME4425/LE4462 is designed for use as a track resistant insulation for the outer layer of Spacer Aerial Cables and as insulation for Partial Insulated Cables. Although it has been used alone as insulation for cables rated at voltages as high as 35kV, it is recommended that a conductor shield such as LE540 be used for cables rated at voltages above 12 kV or where required by the applicable electrical code.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.935 g/ccASTM D1928 C/D 1505
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D2240
Tensile Strength, Yield >= 2000 psiHeat Aging (7 days at 121°C); ASTM D638
 2350 psiAt 20 in/min; ASTM D638
Elongation at Break 255 %Heat Aging (7 days at 121°C); ASTM D412
 300 %At 20 in/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength >= 800 V/milAt 40 mils; ASTM D149
Track Resistance 1.08e+6 secDust and Fog; ASTM D2132
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature >= 180 °C
Front Barrel Temperature >= 160 °C
Die Temperature >= 375 °F
Head Temperature >= 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes
Borealis Borlink™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables
Borealis Borlink™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables
Borealis Visico™/Ambicat™ LE4421/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation

PBOREA205 / 27512

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.