MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin FP5140 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ FP5140 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant with a UL94 flame rating of V1 at 1.5mm NORYL FP5140 resin was designed to have very good dimensional stability with high flow and exhibits good rheological properties, high heat resistance, hydrolysis resistance, and very low density. The combination of these properties makes this material an excellent candidate for Flat Panel TV enclosure applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,High Flow,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Moisture Absorption 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.18 %0.18 %ISO 62-1
Viscosity  15 cP
@Load 1.20 kg,
Temperature 280 °C
15 cP
@Load 2.65 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
 44 cP
@Load 2.16 kg,
Temperature 280 °C
44 cP
@Load 4.76 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 48.0 MPa6960 psi50 mm/min; ISO 527
Tensile Strength, Yield 58.0 MPa8410 psi50 mm/min; ISO 527
Elongation at Break 7.0 %7.0 %50 mm/min; ISO 527
Elongation at Yield 3.5 %3.5 %50 mm/min; ISO 527
Tensile Modulus 2.45 GPa355 ksi1 mm/min; ISO 527
 2.94 GPa426 ksi50 mm/min; ASTM D638
Flexural Strength 87.0 MPa12600 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 - 3.50e+16 ohm-cm3.00e+16 - 3.50e+16 ohm-cmASTM D257
 3.00e+16 - 3.50e+16 ohm-cm3.00e+16 - 3.50e+16 ohm-cmIEC 60093
Surface Resistance 8.00e+13 - 8.50e+13 ohm8.00e+13 - 8.50e+13 ohmASTM D257
 8.00e+16 - 8.50e+16 ohm8.00e+16 - 8.50e+16 ohmROA; IEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 27.5 kV/mm
@Thickness 1.60 mm
699 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
Dissipation Factor  0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
46.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 81.0 °C
@Thickness 3.20 mm
178 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 103 °C217 °FRate B/50; ASTM D1525
 105 °C221 °FRate B/50; ISO 306
 110 °C230 °FRate B/120; ISO 306
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94  V-2
@Thickness >=1.00 mm
V-2
@Thickness >=0.0394 in
UL 94
 V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=2.00 mm
V-0
@Thickness >=0.0787 in
UL 94
Oxygen Index 30 %30 %ISO 4589
Glow Wire Ignition Temperature  700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 240 - 270 °C464 - 518 °F
Zone 2 230 - 260 °C446 - 500 °F
Zone 3 250 - 285 °C482 - 545 °F
Melt Temperature 250 - 285 °C482 - 545 °FInjection Molding
Mold Temperature 40.0 - 65.0 °C104 - 149 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °FInjection Molding
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82301 / 290248

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.