MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® XE 3959 nat PA610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and its eco-profile is very favourable when compared to similar products based on crude oil. The main features of Grilamid XE 3959 natural are:
  • Low volume expansion of tubes under pressure
  • Good cold impact behaviour
  • High heat and chemical resistance
  • Easy processing
Grilamid XE 3959 natural can be processed on standard tube-extrusion lines suitable for polyamides.

Grilamid XE 3959 natural was specially developed for automotive tubing applications for which a high long term usage and peak temperature are required. Grilamid XE 3959 natural has an excellent volume expansion behaviour and is particularly suitable for hydraulic clutch tubes.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Water Absorption 3.3 %ISO 62
Moisture Absorption 1.60 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 70.0 MPaconditioned; ISO 2039-1
 120 MPadry; ISO 2039-1
Tensile Strength at Break 40.0 MPadry; ISO 527-1/-2
 60.0 MPaconditioned; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPaconditioned; ISO 527-1/-2
 60.0 MPadry; ISO 527-1/-2
Elongation at Break >= 50 %dry; ISO 527-1/-2
 >= 50 %conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %dry; ISO 527-1/-2
 18 %conditioned; ISO 527-1/-2
Tensile Modulus 1200 MPaconditioned; ISO 527-1/-2
 2200 MPadry; ISO 527-1/-2
Charpy Impact Unnotched NBdry; ISO 179/1eU
 NBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
conditioned; ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²dry; ISO 179/1eA
 18.0 kJ/m²conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
conditioned; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmdry; IEC 60093
 1.00e+11 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 34.0 kV/mmdry; IEC 60243-1
 34.0 kV/mmconditioned; IEC 60243-1
Comparative Tracking Index 600 Vconditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 130 °Clong term; EMS
 160 °Cshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 150 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Compressed air systems
 Fuel systems
 Hydraulic systems
 Powertrain and Chassis
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Tools & Accessories
ProcessingOther Extrusion
 Profile Extrusion
Product AttributesBio based Polyamide
 High viscosity
Special CharacteristicsHigh impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)
 Light stabilized or stable to light

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® XE 3959 black 9992 PA610
EMS-Grivory Grilamid® TR 90 LXS PAMACM12
EMS-Grivory Grilamid® LV-3H PA12-GF30
EMS-Grivory Grilamid® 2SV-30H nat PA610-GF30
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp

PGRH117 / 156826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.