MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Polymist® F-510 PTFE Powder Lubricant  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); PTFE Powder

Material Notes: Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist powders have been specially produced to provide a finely divided product which will not agglomerate and can easily be dispersed in dry or liquid media. Polymist powders are used as additives in elastomers and plastics where improved lubricity and/or wear resistance is required. In paints and coatings Polymist powders are designed for use as additives where narrow particle size distribution is required and improvements in release, mar resistance, slip, chemical resistance, weatherability, and moisture repelling characteristics are desired. Printing inks use Polymist powders as scuff resistant additives. Polymist powders are used as dry lubricants in machinery where liquid lubricants and/or potential staining cannot be tolerated.

Uses: Thermoplastics, thermoset resins, paints, coatings, printing inks, oils, and greases.

Benefits of Polymist powders are it can be used alone as dry-film lubricants, or as additives in plastics, elastomers and other media; does not agglomerate or lump during handling or processing; inert to practically all chemical solvents; reduces the friction coefficient; improves wear characteristics; UV and weather resistant; improved nonstick and release properties; increased rub resistance; improved corrosion resistance, improved thermal stability; improved thermal stability; improved corrosion resistance; improved thermal stability; excellent electrical insulator; and does not absorb moisture.

Information provided by Solvay Solexis, Inc.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.475 g/cc
Density 2.28 g/cc
Particle Size <= 25 µm
Specific Surface Area 3.0 m²/g
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction <= 0.10
 
Thermal PropertiesOriginal ValueComments
Melting Point 325 - 330 °C
Crystallization Temperature 312 - 318 °C
 
Descriptive Properties
ColorWhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTFEAU03 / 70097

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.