MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
NMG BalCore™ Balsa Wood Block Density 110 kg/m3
Categories: Other Engineering Material; Composite Core Material; Wood and Natural Products; Wood

Material Notes: Very high strength-to-weight ratio and stiffness-to-weight ratio. With its surface specially coated, it can bond with any kinds of resins or adhesives allowing use as a core material for manufacturing sandwich structural products

Information provided by NMG Composites Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.100 - 0.120 g/ccASTM-C271
Water Absorption <= 12 %ISO 3130
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7.40 MPaASTM–C297
Tensile Modulus 2200 MPaASTM–C297
Compressive Strength 6.30 MPaASTM-C365
Compressive Modulus 1990 MPaASTM-C365
Shear Modulus 0.106 GPaASTM-C273
Shear Strength 1.80 MPaASTM-C273
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0480 W/m-KASTM-C177
Maximum Service Temperature, Air 163 °C
Minimum Service Temperature, Air -212 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
Armacell ArmaFORM® FR100 PET foam core
DIAB Rigid Foam IPN 20-649 Type 1
DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density
General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam

PNMG910 / 230587

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.