MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MOL Group TIPELIN H 880 HDPE, Extrusion molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Description: TIPPLEN H 880 is a homopolymer polypropylene with high molecular weight, outstanding mechanical properties and excellent long-term heat stability for extrusion. TIPPLEN H 880 has excellent weldability.

Applications: TIPPLEN H 880 is recommended for extrusion of thick heavy sheets for industrial applications, thin sheets for thermoforming, straps, profiles and pipes.

(1) Average mechanical property values of several measurements carried out on standard injection-molded test specimens prepared in accordance with ISO 294-1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Oxidative Induction Time (OIT) 50 min
@Temperature 210 °C
EN 728
Melt Flow 0.25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
Storage Temperature <= 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 931; ISO 2039-2
Tensile Strength, Yield 40.0 MPa1; ISO 527-1,2
Elongation at Yield 11 %1; ISO 527-1,2
Modulus of Elasticity 1.75 GPa1, in Tension; ISO 527-1,2
Flexural Modulus 1950 MPa1; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²1; ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C1, flatwise; ISO 75-1,2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 255 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOLG045 / 297211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.