MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Purell RP370M Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Purell RP370M is a medium modified polypropylene random copolymer. It does not contain slip or anti-blocking additives. Purell RP370M is typically used by customers for manufacturing of un-oriented cast films and blown film extrusion. It has been reported by customers that Purell RP370M exhibits good processability, and that films produced with Purell RP370M exhibits high clarity and gloss, softness and good heat weldability.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Caps & Closures (Healthcare); Healthcare Applications; Infusion Bags; Medical Film

Market: Healthcare

Processing Method: Cast Film; Injection Molding

Attribute: Autoclavable; Ethylene Oxide Sterilization; Good Optical Properties; Medium Transparency

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 8.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1, -2
Elongation at Break >= 50.0 %>= 50.0 %ISO 527-1, -2
Elongation at Yield 14.0 %14.0 %ISO 527-1, -2
Tensile Modulus 0.850 GPa123 ksiISO 527-1, -2
Charpy Impact, Notched  0.300 J/cm²
@Temperature 0.000 °C
1.43 ft-lb/in²
@Temperature 32.0 °F
ISO 179-1/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C154 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 135 °C275 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9789 / 324724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.