MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV X23040N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X23040N is a highly engineered thermoplastic vulcanizate that can also be used as a materbatch compound in demanding automotive industrial applications. This product is a medium hardness, low density, RoHS compliant grade with a low compression set, good chemical resistance and high temperature performance. It can be easily process by injection molding, extrusion, or thermoforming.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Compression Set; Good Processability; High Heat Resistance: High Tensile Strength; Low Density; Low Specific Gravity; Medium Hardness

Uses: Automotive Applications; Automotive Interior Parts; Constant Velocity Joint Boots; Gaskets; Industrial Applications; Profiles; Seals

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Thermoforming

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Viscosity 360 cP
@Shear Rate 206 1/s,
Temperature 200 °C
360 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  35
@Time 5.00 sec
35
@Time 0.00139 hour
Extruded; ISO 868
 37
@Time 5.00 sec
37
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 2.10 MPa305 psiFlow; ISO 37
 3.90 MPa566 psiAcross Flow; ISO 37
Tensile Stress at Strain  0.903 MPa
@Strain 100 %
131 psi
@Strain 100 %
Across Flow; ISO 37
 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 210 %210 %Flow; ISO 37
 710 %710 %Across Flow; ISO 37
Tear Strength 16.0 kN/m91.0 pliMethod Ba, Angle (Unnicked), Across Flow; ISO 34-1
Compression Set  20 %
@Temperature 22.8 °C,
Time 79200 sec
20 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 221 °C360 - 430 °FMelt, Injection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Zone 1 182 - 204 °C360 - 400 °FExtrusion
Zone 2 182 - 204 °C360 - 400 °FExtrusion
Zone 3 188 - 210 °C370 - 410 °FExtrusion
Zone 4 188 - 210 °C370 - 410 °FExtrusion
Die Temperature 193 - 216 °C380 - 420 °FExtrusion
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers EFLEX® V2045 SEBS/TPV
Chengdu Polyster 4502 High Performance Grade TPV
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

PTEKNQ1232 / 237723

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.