MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax TYC 568X C1 BLACK Polypropylene, Impact Modified, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced, Impact Modified

Material Notes: HIFAX TYC 568X C1 Black is a mineral reinforced, impact modified polypropylene copolymer for injection molding. It combines very high rigidity with a low coefficient of linear thermal expansion (CLTE) and very good processability for body panel applications. The grade has been specifically designed for molding of large complex parts that require good dimensional.

Status: Commercial – Active

Availability: Asia-Pacific

Application: Body Panels; Exterior Automotive Applications

Market: Automotive

Processing Method: Injection Molding

Attribute: Good Dimensional Stability; Good Impact Resistance; Good Processability; Impact Modified; Low Shrinkage; Paintable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183-1/A
Melt Flow 25.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 20.0 MPaISO 527-1, -2
Flexural Modulus 3000 MPaTech. A; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 45.0 µm/m-°CISO 11359-1, -2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9181 / 324116

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.