Kao-Tex Textile 2000 Cloths are made from alumina-silica ceramic fibers that are reinforced with an organic carrier fiber for added strength and stability, making them an excellent choice for industrial applications. The nature of the engineered yarns and weave types, provide excellent strength, resulting in a physically resilient material well suited to high temperature industrial applications. Applications: - Welding, Fire, Oven and Drop curtains
- Stress Relieving blankets
- Fire and Heat barriers
- Removable Insulation
- Lagging
- Fabric Expansion joints
- Gasketing and Sealing
- Gloves and Mittens
Information provided by Morgan Advanced Materials |