MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 ISO Grade 150 Circulating Oil
Categories: Fluid; Lubricant

Material Notes: Circulating Oil is a high-quality, rust-inhibited mineral oil specially developed for the lubrication of conveyor and crusher bearings in copper crushing mills. Circulating Oil is formulated to provide protection against rust and corrosion and resistance to foaming. It has excellent water-separating properties to minimize the formation of emulsions in circulating systems subject to contamination with large quantities of water, minerals, dirt and scale.

Applications:

  • Ball mills, cement mills, hot and cold strip mills, plate mills
  • Conveyor bearings in mining applications
  • Plain and rolling-element bearings in ferrous and non-ferrous mills
  • Circulating systems where water contamination is a problem
  • Large, slow-speed bearings in mixers and mills

    Features/Benefits:

    • Excellent water-separating properties to minimize the formation of emulsions
    • Good oxidation resistance
    • Protects against rust and corrosion
    • Good foam resistance

    Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.878 g/cc0.878 g/cc
Density 0.876 g/cc0.0316 lb/in³
Viscosity Measurement 9595Index
Saybolt Viscosity at 100°F 805 SUS805 SUS
Saybolt Viscosity at 210°F 78.5 SUS78.5 SUS
Kinematic Viscosity at 40°C (104°F) 153 cSt153 cSt
Kinematic Viscosity at 100°C (212°F) 14.7 cSt14.7 cSt
ASTM Color 2.02.0ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0500.050[mg KOH/g]; ASTM D974
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Flash Point 277 °C531 °FCOC
 
Descriptive Properties
Demulsibility5 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5164 / 198417

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.