MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shanghai Potomer CPE-135APT Chlorinated Polyethylene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Chlorosulfonated Polyethylene Rubber

Material Notes: Properties: Chlorinated Polyethylene CPE-135APT is a new brand for plastic modification. Chlorinated Polyethylene CPE-135APT main application is to increase plastification of CPE and make CPE better adapted to the original customers who use ACR and MBS as modifiers.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³
Volatiles <= 0.30 %<= 0.30 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A <= 65<= 65
Tensile Strength >= 6.00 MPa>= 870 psi
Elongation at Break >= 600 %>= 600 %
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion <= 2.00 J/g<= 0.860 BTU/lb
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca <= 2.1 %<= 2.1 %
Chlorine, Cl 34 - 36 %34 - 36 %
 
Descriptive Properties
Content<30 pieces/200gImpurity particles
Sieving Remainder<2%0.8mm sieve
Time of stability>8 min165°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM102 / 284548

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.