MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ LUBRICOMP™ Compound OCL36A Polyphenylene Sulfide, Branched (PPS, Branched) (Europe)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP LUBRICOMP OCL36A compound is based on Polyphenylene Sulfide (PPS) - branched resin containing 30% carbon fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ISO 1183
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0300 %0.0300 %23°C / 50% RH; ISO 62
Viscosity 4.0 - 6.0 cP
@Load 5.00 kg,
Temperature 315 °C
4.0 - 6.0 cP
@Load 11.0 lb,
Temperature 599 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0019 cm/cm0.0019 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0095 cm/cm0.0095 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 153 MPa22200 psi5 mm/min; ISO 527
Elongation at Break 0.70 %0.70 %5 mm/min; ISO 527
Tensile Modulus 25.0 GPa3630 ksi1 mm/min; ISO 527
Flexural Strength 217 MPa31500 psibreak, 2mm/min; ISO 178
 261 MPa37900 psiyield, 2 mm/min; ISO 178
 66.0 MPa
@Temperature 200 °C
9570 psi
@Temperature 392 °F
yield, 2 mm/min; ISO 178
 94.0 MPa
@Temperature 150 °C
13600 psi
@Temperature 302 °F
yield, 2 mm/min; ISO 178
 118 MPa
@Temperature 120 °C
17100 psi
@Temperature 248 °F
yield, 2 mm/min; ISO 178
 212 MPa
@Temperature 80.0 °C
30700 psi
@Temperature 176 °F
yield, 2 mm/min; ISO 178
Flexural Modulus 21.2 GPa3070 ksi2 mm/min; ISO 178
 6.10 GPa
@Temperature 200 °C
885 ksi
@Temperature 392 °F
2 mm/min; ISO 178
 7.90 GPa
@Temperature 150 °C
1150 ksi
@Temperature 302 °F
2 mm/min; ISO 178
 10.2 GPa
@Temperature 120 °C
1480 ksi
@Temperature 248 °F
2 mm/min; ISO 178
 20.6 GPa
@Temperature 80.0 °C
2990 ksi
@Temperature 176 °F
2 mm/min; ISO 178
Flexural Strain at Break 1.3 %1.3 %2 mm/min; ISO 178
 1.3 %
@Temperature 80.0 °C
1.3 %
@Temperature 176 °F
2 mm/min; ISO 178
 2.3 %
@Temperature 120 °C
2.3 %
@Temperature 248 °F
2 mm/min; ISO 178
 2.4 %
@Temperature 150 °C
2.4 %
@Temperature 302 °F
2 mm/min; ISO 178
 2.4 %
@Temperature 200 °C
2.4 %
@Temperature 392 °F
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) 26.0 kJ/m²12.4 ft-lb/in²80*10*4; ISO 180/1U
 23.0 kJ/m²
@Temperature -40.0 °C
10.9 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.390.39ASTM D3702 Modified: Manual
K (wear) Factor 38.3 x 10-8 mm³/N-M19.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10 - 1000 ohm10 - 1000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 3.00 µm/m-°C
@Temperature 23.0 - 60.0 °C
1.67 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 49.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.2 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Specific Heat Capacity 1.633 J/g-°C0.3903 BTU/lb-°FASTM E1269
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°FASTM D5930
Deflection Temperature at 0.46 MPa (66 psi) 278 °C532 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 
Processing PropertiesMetricEnglishComments
Zone 2 320 - 330 °C608 - 626 °F
Zone 3 330 - 345 °C626 - 653 °F
Melt Temperature 315 - 320 °C599 - 608 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80915 / 288862

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.